104 / 2016-11-14 11:11:23
Comparative Study on the Corrosion and Freeze-thaw Durability of Aircraft Deicer and Airfield Pavement Deicer
11828,11829,11830,1357,11831
摘要待审
During the corrosion cycle of 50 day, for the surface of OPC in the aircraft deicer it has net cracks, while in the airport pavement deicer it doesn’t show a tendency to crack but having white matter. Under the coupling effect of corrosion and freeze-thaw, the surface properties of the aircraft deicer are better than that of the airport pavement deicer. Under the simple corrosion cycle or coupling action of corrosion and freeze-thaw for the deterioration degree of mechanical properties (compressive strength and flexural strength) of airport pavement concrete the airport pavement deicer is larger than the aircraft deicer. Finally, no matter whether the aircraft deicer or airfield pavement deicer, the coupling effect of corrosion and freeze-thaw has a significant influence on the concrete degradation of the airport deicing plateau.
重要日期
  • 12月29日

    2016

    会议日期

  • 12月10日 2016

    初稿截稿日期

  • 12月13日 2016

    终稿截稿日期

  • 12月29日 2016

    注册截止日期

主办单位
中国自然资源学会
中国地质大学(北京)人文经管学院
湖北省众科地质与环境技术服务中心
承办单位
中国地质调查局发展研究中心
湖北省众科地质与环境技术服务中心
北京土人咨询服务有限公司
联系方式
移动端
在手机上打开
小程序
打开微信小程序
客服
扫码或点此咨询